Specific Process Knowledge/Thin film deposition/Deposition of Platinum: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 32: | Line 32: | ||
|- | |- | ||
| Layer thickness | | Layer thickness | ||
|10Å to 5000Å | |10Å to 5000Å* | ||
|10Å to 5000Å | |10Å to 5000Å* | ||
|10Å to 5000Å | |10Å to 5000Å | ||
|- | |- | ||
| Line 42: | Line 42: | ||
|- | |- | ||
|} | |} | ||
'''*''' ''For thicknesses above 200 nm permission is required from Thin Film group.'' | |||
Revision as of 14:47, 7 March 2014
Feedback to this page: click here
Platinum deposition
Platinum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | Sputter deposition (Lesker) | |
|---|---|---|---|
| Batch size |
|
|
|
| Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 5000Å* | 10Å to 5000Å* | 10Å to 5000Å |
| Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s | ? Å/s to ? Å/s |
* For thicknesses above 200 nm permission is required from Thin Film group.