Specific Process Knowledge/Lithography/Strip: Difference between revisions
Appearance
| Line 229: | Line 229: | ||
=Acetone Strip= | =Acetone Strip= | ||
[[Image:Lift-off wet bench.JPG|300x300px|thumb|Acetone strip bench in D-3]] | |||
{| border="1" cellspacing="0" cellpadding="4" align="right" | {| border="1" cellspacing="0" cellpadding="4" align="right" | ||
|[[Image:Acetone_rough.jpg|150x150px|thumb|Acetone bath "rough" for removing most of the resist]] | |[[Image:Acetone_rough.jpg|150x150px|thumb|Acetone bath "rough" for removing most of the resist]] | ||