==RCA cleaning== | ==RCA cleaning== | ||
[[Image:RCA-bænk_RR2_0.JPG|300x300px|thumb|RCA bench: positioned in cleanroom | [[Image:RCA-bænk_RR2_0.JPG|300x300px|thumb|RCA bench: positioned in cleanroom B1. <br /> RCA1 - RCA2 - HF - BHF(pre-dep wafers)]] | ||
The RCA clean is used for cleaning the wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). | The RCA clean is used for cleaning the wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). | ||