Jump to content

Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions

Kabi (talk | contribs)
No edit summary
Kabi (talk | contribs)
Line 13: Line 13:
Both solutions are used in the Aluminium etch bath shown to the right. It must be written on which one is in. Solution no. 1 is the most used solution for etching aluminium. Solution no. 2 is primarily for etching aluminium mixed with a small percentage of silicon.  
Both solutions are used in the Aluminium etch bath shown to the right. It must be written on which one is in. Solution no. 1 is the most used solution for etching aluminium. Solution no. 2 is primarily for etching aluminium mixed with a small percentage of silicon.  


'''The user manual and contact information can be found in LabManager:'''
<!-- remember to remove the type of documents that are not present -->
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=68 Al-etch info page in LabManager]


===Comparing the two solutions===
===Comparing the two solutions===