Specific Process Knowledge/Thin film deposition/MVD: Difference between revisions
Appearance
| Line 3: | Line 3: | ||
== The Molecular Vapor Deposition tool == | == The Molecular Vapor Deposition tool == | ||
[[image:Mvd.jpg|200x200px|right|thumb|The MVD is located in cleanroom | [[image:Mvd.jpg|200x200px|right|thumb|The MVD is located in cleanroom D-3]] | ||
The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At Danchip the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps. | The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At Danchip the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps. | ||
Revision as of 15:32, 17 February 2014
Feedback to this page: click here
The Molecular Vapor Deposition tool

The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At Danchip the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps.
The user manual, user APV, and contact information can be found in LabManager:
Process information
| Purpose |
| ||
|---|---|---|---|
| Vapor sources | Line
|
Chemical
| |
| Performance | Contact angle |
110° (water) | |
| Process parameters | Base pressure |
20 mTorr | |
| Chamber temperature |
35°C | ||
| Chamber volume |
Approx. 3 liters | ||
| Substrates | Substrate size |
1" to 8" Smaller samples may be processed if fixed to a carrier | |
| Allowed materials |
All cleanroom materials | ||
| Batch |
One sample at a time Two 4" or 6" wafers may be processed simultaneously using cassettes | ||