The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters. | The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters. | ||
'''The user manual(s), user APV(s) and contact information can be found in LabManager:''' | '''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:''' | ||
<!-- remember to remove the type of documents that are not present --> | <!-- remember to remove the type of documents that are not present --> | ||
Revision as of 14:43, 7 February 2014
Feedback to this page: click here
TPT Wire Bonder

Packlab, Building 347, 2nd floor
The TPT Wire Bonder is bought i 2007. Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
Ball Wire Bonder K&S 4524

Packlab, Building 347, 2nd floor

The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
| Equipment | TPT Wire Bonder | Ball Wire Bonder | |
|---|---|---|---|
| Purpose |
|
| |
| Performance |
|
| |
| Substrates | Allowed materials |
| |