Jump to content

Specific Process Knowledge/Back-end processing/Wire Bonder: Difference between revisions

From LabAdviser
Kabi (talk | contribs)
Kabi (talk | contribs)
Line 14: Line 14:


==Ball Wire Bonder K&S 4524==
==Ball Wire Bonder K&S 4524==
[[Image:TPTwirebonder_wedge_ball.jpg|300x300px|thumb|Wire bondings: Left: wedge bonding - Right: ball bonding]]
[[Image:K&S_4524_ball_wire-bonder.jpg|300x300px|thumb|The Ball Wire Bonder K&S 4524, <br/> Packlab, Building 347, 2nd floor]]


The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.  
The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.  
Line 20: Line 22:
<!-- remember to remove the type of documents that are not present -->
<!-- remember to remove the type of documents that are not present -->


[[Image:K&S_4524_ball_wire-bonder.jpg|300x300px|thumb|The Ball Wire Bonder K&S 4524, <br/> Packlab, Building 347, 2nd floor]]


<!-- give the link to the equipment info page in LabManager: -->
<!-- give the link to the equipment info page in LabManager: -->

Revision as of 16:39, 5 February 2014

Feedback to this page: click here

TPT Wire Bonder

TPT Wire Bonder,
Packlab, Building 347, 2nd floor

The TPT Wire Bonder is bought i 2007. Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder.

The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:

TPT Wire Bonder

Ball Wire Bonder K&S 4524

Wire bondings: Left: wedge bonding - Right: ball bonding
The Ball Wire Bonder K&S 4524,
Packlab, Building 347, 2nd floor

The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.

The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:


Ball Wire Bonder


Equipment performance and process related parameters

Equipment TPT Wire Bonder Ball Wire Bonder
Purpose
  • Al and Au 25µm wire bonding
  • Wedge and ball wire bonding
  • Au ribbon (100x20µm) bonding
    (we have tools and wire but it has not been tested)
  • Au 25µm wire bonding
  • Ball wire bonding
Performance
  • Manual operation
  • Wedge bonding:
    • recommended min. bonding area 200 µm
  • Ball bonding:
    • recommended min. bonding area 200 µm
    • recommended temperature 120 oC.
  • Semi-automatic and manual operation
  • Bond placement laser pointer
  • recommended min. bonding area 100 µm
  • recommended temperature 120 oC.
Substrates Allowed materials
  • Should be able to withstand the wire bonding temperature
  • Typical materials are: Alumina (Al2O3), AluminumNitride (AlN), std. circuit boards (FR4)