==Apox furnace (D1)== | ==Apox furnace (D1)== | ||
[[Image:APOX.JPG|thumb|300x300px|Apox furnace (D1): positioned in the | [[Image:APOX.JPG|thumb|300x300px|Apox furnace (D1): positioned in the A5 room]] | ||
The APOX furnace (D1) is a Tempress horizontal furnace for oxidation silicon wafers. This furnace is dedicated for oxidation of new and clean Si wafers to form apox layers which is a very thick wet thermal oxide grown at 1075<sup>o</sup>C. Running a batch of apox wafers (oxide thickness > 5µm) can take several weeks, depending on how thick an apox layer that is required. | The APOX furnace (D1) is a Tempress horizontal furnace for oxidation silicon wafers. This furnace is dedicated for oxidation of new and clean Si wafers to form apox layers which is a very thick wet thermal oxide grown at 1075<sup>o</sup>C. Running a batch of apox wafers (oxide thickness > 5µm) can take several weeks, depending on how thick an apox layer that is required. | ||