Specific Process Knowledge/Etch: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
==Comparing wet etch and dry etch== | |||
Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate. | Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate. | ||
Advantages of wet chemistry over dry etch techniques are: | Advantages of wet chemistry over dry etch techniques are: | ||
*A often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials. | *A often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials. | ||
* | *Time saving: You can often etch 25 wafers at a time in wet chemistry where as dry etch equipment can only handle one wafer at a time. | ||
== Choose material to be etched == | == Choose material to be etched == | ||