Jump to content

Specific Process Knowledge/Thermal Process/C4 Aluminium Anneal furnace: Difference between revisions

Mdyma (talk | contribs)
Mdyma (talk | contribs)
Line 37: Line 37:
|style="background:LightGrey; color:black"|Gas flows
|style="background:LightGrey; color:black"|Gas flows
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*N<sub>2</sub>: 5 slm
*N<sub>2</sub>: 10 slm
*O<sub>2</sub>: 5 slm
*O<sub>2</sub>: 10 slm
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates