Specific Process Knowledge/Thermal Process/C4 Aluminium Anneal furnace: Difference between revisions
Appearance
| Line 37: | Line 37: | ||
|style="background:LightGrey; color:black"|Gas flows | |style="background:LightGrey; color:black"|Gas flows | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*N<sub>2</sub>: 5 | *N<sub>2</sub>: 5 slm | ||
*O<sub>2</sub>: 5 | *O<sub>2</sub>: 5 slm | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | ||
Revision as of 10:49, 14 January 2014
Feedback to this page: click here
Aluminium Anneal furnace (C4)

The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for oxidation and annealing of silicon wafers with aluminium.
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
- Annealing: look at the Annealing page
| Purpose |
|
|
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
|