The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium. | The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for oxidation and annealing of silicon wafers with aluminium. | ||
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace. | This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace. | ||
Revision as of 15:53, 10 January 2014
Feedback to this page: click here
Aluminium Anneal furnace (C4)

The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for oxidation and annealing of silicon wafers with aluminium.
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
- Annealing: look at the Annealing page
| Purpose |
|
|
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate materiasl allowed |
|