Specific Process Knowledge/Characterization/Drop Shape Analyzer: Difference between revisions
Appearance
| Line 14: | Line 14: | ||
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=240 Drop Shape Analyzer in LabManager] | [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=240 Drop Shape Analyzer in LabManager] | ||
==An overview of the performance of the | ==An overview of the performance of the Drop Shape Analyzer== | ||
{| border="2" cellspacing="0" cellpadding="10" | {| border="2" cellspacing="0" cellpadding="10" | ||
|- | |- | ||
!style="background:silver; color:black;" align="left"|Purpose | !style="background:silver; color:black;" align="left"|Purpose | ||
|style="background:LightGrey; color:black"| | |style="background:LightGrey; color:black"|Imaging and analysis of of the shape of the interface between liquid and air||style="background:WhiteSmoke; color:black"| | ||
*Measurement of | *Measurement of contact angle between sample surface and liquid | ||
* | *Measurement of surface tension of liquid | ||
|- | |- | ||
!style="background:silver; color:black" align="left"|Performance | !style="background:silver; color:black" align="left"|Performance | ||
Revision as of 14:39, 10 January 2014
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
The Drop Shape Analyzer
The Krüss DSA 100S Drop Shape Analyzer will analyze the shape a drop of liquid on a surface, or suspended from a needle, in order to calculate the contact angle, or the surface tension, respectively.

The user manual, user APV(s), technical information, and contact information can be found in LabManager:
Drop Shape Analyzer in LabManager
An overview of the performance of the Drop Shape Analyzer
| Purpose | Imaging and analysis of of the shape of the interface between liquid and air |
|
|---|---|---|
| Performance | Thin film materials that can be measured |
Film with a refractive index of less than 2.02 and that are transparent to the light in the given wavelength range ex:
|
| Film thickness range |
| |
| Film thickness accuracy |
| |
| Index accuracy |
| |
| Process parameter range | Wavelength range |
Can operate at two different wavelength:
|
| Substrates | Batch size |
|
| Substrate material allowed |
|