Specific Process Knowledge/Thermal Process/C4 Aluminium Anneal furnace: Difference between revisions
Appearance
| Line 6: | Line 6: | ||
The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium. | The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium. | ||
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that contain aluminium. Check the | This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that contain aluminium. Check the cross contamination information in LabManager for more information. | ||
'''The user manual, technical information and contact information can be found in LabManager:''' | '''The user manual, technical information and contact information can be found in LabManager:''' | ||
Revision as of 15:57, 9 January 2014
Feedback to this page: click here
Aluminium Anneal furnace (C4)

The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium.
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that contain aluminium. Check the cross contamination information in LabManager for more information.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
- Annealing: look at the Annealing page
| Purpose | Annealing | Annealing of wafers containing aluminium. |
|---|---|---|
| Performance | Film thickness | |
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|