Specific Process Knowledge/Thermal Process/C3 Anneal-bond furnace: Difference between revisions
Appearance
| Line 23: | Line 23: | ||
|- | |- | ||
!style="background:silver; color:black;" align="center"|Purpose | !style="background:silver; color:black;" align="center"|Purpose | ||
|style="background:LightGrey; color:black"|Oxidation | |style="background:LightGrey; color:black"| | ||
*Oxidation of Si wafers | |||
*Annealing of processed wafer, eg. bonded wafers | |||
|style="background:WhiteSmoke; color:black"|Oxidation: | |style="background:WhiteSmoke; color:black"|Oxidation: | ||
*Dry | *Dry | ||
| Line 31: | Line 33: | ||
|style="background:LightGrey; color:black"|Film thickness | |style="background:LightGrey; color:black"|Film thickness | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Dry SiO<sub>2</sub>: 50 Å to ~2000 Å (takes too long to | *Dry SiO<sub>2</sub>: 50 Å to ~2000 Å (it takes too long to grow a thicker oxide) | ||
*Wet SiO<sub>2</sub>: 50 Å to ~5 µm (takes too long to | *Wet SiO<sub>2</sub>: 50 Å to ~5 µm (it takes too long to grow a thicker oxide) | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range | !style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range | ||
| Line 45: | Line 47: | ||
|style="background:LightGrey; color:black"|Gas flows | |style="background:LightGrey; color:black"|Gas flows | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*N<sub>2</sub>:5 sccm | *N<sub>2</sub>: 5 sccm | ||
*O<sub>2</sub>:5 sccm | *O<sub>2</sub>: 5 sccm | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | ||
Revision as of 15:16, 9 January 2014
Feedback to this page: click here
Anneal-bond furnace (C3)
The Anneal-bond furnace (C3) is a Tempress horizontal furnace for oxidation and annealing of new and processed (bonded) silicon wafers.
This furnace is the third furnace tube in the furnace C-stack positioned in cleanroom 2.
In this furnace it is allowed oxidize and anneale wafers without doing a RCA clean first. Also bonded wafers comming directly from the EVG NIL (assuming they were very clean when entering EVG NIL and not contain any metal). Check the cross contamination information in LabManager can enter the furnace. Check the cross contamination information in LabManager.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
| Purpose |
|
Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|