Specific Process Knowledge/Lithography/NanoImprintLithography: Difference between revisions
Appearance
| Line 10: | Line 10: | ||
'''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach= | '''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=153 LabManager]''' | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 12:48, 25 November 2013
EVG NIL

Feedback to this section: EVG NIL click here
The EVG NIL is a system for imprinting in polymers (Hot Embossing), and for bonding on wafer scale. 3 different types of bonding can be done: Anodic, Eutectic and Fusion. Furthermore it is possible to align the wafers one wishes to bond. In principle it is also possible to align the substrate and stamp before imprint, but it is much more difficult.
It is possible to fill bonded cavities with a desired gas. At the moment we have SF6 on the system, but if you would like another one, please contact Rune Christiansen.
The user manual, user APV, and contact information can be found in LabManager