==Cleaning of wafers or masks==
==Cleaning of wafers or masks==
[[Image:7-up_RR3.jpg|300x300px|right|thumb|7-up 4": positioned in cleanroom 3<br\> -Up to 19 wafers of 4" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
 
Cleaning of wafers or masks with sulphuric acid can be done either in a dedicated tank "7-up" or in the fume hood in a beaker "Piranha"
Cleaning of wafers or masks with sulphuric acid can be done either in a dedicated tank "7-up" or in the fume hood in a beaker "Piranha"
Both 7-up and Piranha removes heavy organics.  
Both 7-up and Piranha removes heavy organics.  
Always use one of these after KOH to remove alkali ions before further processing. 7-up and Piranha are also used as cleaning solutions after stripping resist.  
Always use one of these after KOH to remove alkali ions before further processing. 7-up and Piranha are also used as cleaning solutions after stripping resist.  


[[Image:7-up_6inch.jpg|300x300px|right|thumb|7-up 6" in cleanroom 4. <br\> -Up to 25 wafers of 4" or 6" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
[[Image:7-up_Mask.jpg|300x300px|right|thumb|7-up for masks and glass wafers positioned in cleanroom 4:<br\> -Up to 25 glass wafers of 4" at a time or 4 masks.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi, glass, chromium]]
[[Image:7-up_RR3.jpg|300x300px|right|thumb|7-up 4": positioned in cleanroom 3<br\> -Up to 19 wafers of 4" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]


===Comparing data for "7-up" and Piranha===
===Comparing data for "7-up" and Piranha===
Line 55: Line 58:
|-
|-
|}
|}
[[Image:7-up_6inch.jpg|300x300px|right|thumb|7-up 6" in cleanroom 4. <br\> -Up to 25 wafers of 4" or 6" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
[[Image:7-up_Mask.jpg|300x300px|right|thumb|7-up for masks and glass wafers positioned in cleanroom 4:<br\> -Up to 25 glass wafers of 4" at a time or 4 masks.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi, glass, chromium]]