Al test
==Etching of Aluminium==
Etching of aluminium is done wet at Danchip. We have two different solutions:
 
(1) H<math>_2</math>O:H<math>_3</math>PO<math>_4</math>  1:2 at 50 <sup>o</sup>C
(2) Pre-mixed etch solution: PES 77-19-04 at 20 <sup>o</sup>C