Jump to content

Specific Process Knowledge/Thin film deposition: Difference between revisions

From LabAdviser
Bghe (talk | contribs)
Bghe (talk | contribs)
Line 96: Line 96:
{| {{table}}
{| {{table}}
| align="left" valign="top"  style="background:LightGray"|''' Dielectrica'''
| align="left" valign="top"  style="background:LightGray"|''' Dielectrica'''
| align="left" valign="top" style="background:#f0f0f0;"|''' Semicondutors'''
| align="left" valign="top" style="background:#DCDCDC;"|''' Semicondutors'''
| align="left" valign="top" style="background:LightGray"|''' Metals'''
| align="left" valign="top" style="background:LightGray"|''' Metals'''
| align="left" valign="top" style="background:#f0f0f0;"|''' Alloys'''
| align="left" valign="top" style="background:#DCDCDC;"|''' Alloys'''
| align="left" valign="top" style="background:LightGray"|''' Polymers'''
| align="left" valign="top" style="background:LightGray"|''' Polymers'''
|-valign="top"
|-valign="top"
Line 105: Line 105:
[[/Deposition of Silicon Oxide|Silicon Oxide]]<br/>
[[/Deposition of Silicon Oxide|Silicon Oxide]]<br/>
[[/Deposition of Titanium Oxide|Titanium Oxide]]<br/>
[[/Deposition of Titanium Oxide|Titanium Oxide]]<br/>
|
|style="background: #DCDCDC"|
[[/Deposition of Silicon|Silicon]]
[[/Deposition of Silicon|Silicon]]
|style="background: LightGray"|
|style="background: LightGray"|
Line 122: Line 122:
[[/Deposition of Platinum|Platinum]]<br/>
[[/Deposition of Platinum|Platinum]]<br/>
[[/Deposition of Gold|Gold]]<br/>
[[/Deposition of Gold|Gold]]<br/>
|
|style="background: #DCDCDC"|
[[/Deposition of TiW|TiW]] alloy (10%/90% by weight) <br/>
[[/Deposition of TiW|TiW]] alloy (10%/90% by weight) <br/>
[[/Deposition of NiCr|NiCr]] alloy  <br/>
[[/Deposition of NiCr|NiCr]] alloy  <br/>

Revision as of 16:02, 14 October 2013

3rd Level - Material/Methode

Feedback to this page: click here


Choose material to deposit

Dielectrica

Metals/elements

Period/Group

IVB VB VIB VIIIB IB IIIA IVA
3 . . . . . 13 Al Aluminium 14 Si Silicon
4 22 Ti Titanium . 24 Cr Chromium 28 Ni Nickel 29 Cu Copper . 32 Ge Germanium
5 . . 42 Mo Molybdenum 46 Pd Palladium 47 Ag Silver . 50 Sn Tin
6 . 73 Ta Tantalum 74 W Tungsten 78 Pt Platinum 79 Au Gold . .

Alloys


Polymers

  • SU8
  • Antistiction coating
  • Topas
  • PMMA

Choose deposition equipment


Section under construction

Dielectrica Semicondutors Metals Alloys Polymers

Silicon Nitride - and oxynitride
Silicon Oxide
Titanium Oxide

Silicon

Aluminium
Titanium
Chromium
Nickel
Copper
Germanium
Molybdenum
Palladium
Silver
Tin
Tantalum
Tungsten
Platinum
Gold

TiW alloy (10%/90% by weight)
NiCr alloy
AlTi alloy

SU8
Antistiction coating
Topas
PMMA