DTU Danchip has a stock of silicon and glass wafers; the most used of these wafers are located on the wafershelves in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=list&page_id=16| wafer shop] in LabManager. The Price can also be found in the wafer shop. | DTU Danchip has a stock of silicon and glass wafers; the most used of these wafers are located on the wafershelves in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=list&page_id=16| wafer shop] in LabManager. The Price can also be found in the wafer shop. | ||
Revision as of 13:52, 11 October 2013
Feedback to this page: click here
Wafer Information
DTU Danchip has a stock of silicon and glass wafers; the most used of these wafers are located on the wafershelves in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the wafer shop in LabManager. The Price can also be found in the wafer shop.
The waferbox name consists typically of a few letters and a number, eg OP337:
| waferbox name OP337 | ||
| O | P | 337 |
|---|---|---|
| Indicates the company where the wafers are bought | Type of doping in the wafer | shipment number |
Wafers available in DTU Danchips cleanroom
| Wafers available in the cleanroom | |||||
| Shelf | Size | Type | Thickness | Resistivity | |
|---|---|---|---|---|---|
| SSP (single side polished) | bottom | 2" | P | 500 µm | 1-20 Ωcm |
| SSP (single side polished) | bottom | 4" | N+P | 525 µm | 1-20 Ωcm |
| SSP (single side polished) | top | 6" | N or P | 625 µm | 1-20 Ωcm |
| DSP (double side polished) | middle | 4" | N+P | 350 µm | 1-20 Ωcm |
| preprocessed | top | 4" and 6" | |||
| Boron glasswafers | middle | 4" | 1 mm | ||
Wafer boxes and single wafer carriers
New clean wafer boxes and single wafer carriers can be found in the gowning area. Ask DTU Danchip personnel for help if stock is low.