Dry oxide:
The thickness and the time it takes to grow the oxide often decides if a dry or wet oxidation is choosen.


Wet oxide with O2 and H2
Dry oxide is used from 5nm - 200nm.
Furnace:A1,A3,C1,C2,C3.


Wet oxide H2O in a bobler
Wet oxide with O2 and H2:
Furnace:A1,A3.
 
Wet oxide H2O in a bobler:
Furnace:C1,C2,C3.

Revision as of 15:08, 2 January 2008

The thickness and the time it takes to grow the oxide often decides if a dry or wet oxidation is choosen.

Dry oxide is used from 5nm - 200nm. Furnace:A1,A3,C1,C2,C3.

Wet oxide with O2 and H2: Furnace:A1,A3.

Wet oxide H2O in a bobler: Furnace:C1,C2,C3.