Jump to content

Specific Process Knowledge/Back-end processing/Polymer Injection Molder: Difference between revisions

From LabAdviser
Choi (talk | contribs)
No edit summary
Jehan (talk | contribs)
mNo edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:CustomerSupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polymer_Injection_Molder click here]'''
'''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polymer_Injection_Molder click here]'''


== Polymer injection molding ==
== Polymer injection molding ==

Revision as of 15:43, 4 October 2013

Feedback to this page: click here

Polymer injection molding

Injection molding machine in the basement under the cleanroom

The injection molder at Danchip is an Engel Victory Tech 80/45. It is a hydraulic machine capable of up to 450 kN of clamping force.

The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:


Polymer injection molding Info on LabManager

Process information

There are no standard processes on the injection molder, since the type of process chosen and process parameters will depend on which polymer that will be used and what type of pattern that is to be replicated during the molding process.

At Danchip the following polymers are used routinely:

Topas 5013L-10
Topas 8007S-04

Some other polymers are used occasionally, such as Polypropylene and Polystyrene. Other polymers can be used after approval and small batches of other polymers are available. Please ask Danchip for details.

Generally two different types of processes are run at Danchip: Constant temperature processes and variotherm processes. An overview of these two processes are given in the table below.

Equipment performance and process related parameters

Parameter Value
Processing temperatures Mold

Up to 160*C

Barrel

Absolute max: 350*C

Processing temperatures Temperature

Up to 160*C

Barrel

Absolute max: 350*C

Molding parameters Injection speed

Up to 53 cm3/s

Injection pressure

Up to 2200 bar

Switch-over point

Time, pressure, volumen or external signal