'''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=188 LabManager]'''
'''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=188 LabManager]'''


<br clear="all" />
=== Equipment performance and process related parameters ===
{| border="2" cellspacing="0" cellpadding="2"
!style="background:silver; color:black;" align="center" width="60"|Purpose
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black"|
*Spin coating and soft baking UV sensative resists
*Spin coating and soft baking E-beam resists
|-
!style="background:silver; color:black;" align="center" width="60"|Resist
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black" align="center"|
* AZ5214E
* AZ4562
* E-beam resists
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Performance
|style="background:LightGrey; color:black"|Coating thickness
|style="background:WhiteSmoke; color:black" align="center"|
* AZ5214E 1-4,2 µm
* AZ4526 6,2-25 µm
* E-beam resits 0,1-1 µm
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameters
|style="background:LightGrey; color:black"|Spin speed
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
100 - 5000 rpm
|-
|style="background:LightGrey; color:black"|Spin acceleration
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
100 - 10000 rpm/s
|-
|style="background:LightGrey; color:black"|Hotplate temperature
|style="background:WhiteSmoke; color:black" align="center"|
* 90°C for softbaking of AZ5214E resist
* 100°C for softbaking of AZ4562 resist
* 110°C for reverse baking of AZ5214E resits
* 180°C for softbaking of e-beam resits
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
|style="background:LightGrey; color:black"|Substrate size
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
* 50 mm wafers
* 100 mm wafers
* 150 mm wafers
|-
| style="background:LightGrey; color:black"|Allowed materials
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
All cleanroom materials except III-V materials
|-
|style="background:LightGrey; color:black"|Batch
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
1 - 24
|-
|}


<br clear="all" />