Ething of Titanium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with [[Specific Process Knowledge/Etch/ICP Metal Etcher|ICP]] using Chlorine chemistry or with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | Ething of Titanium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with [[Specific Process Knowledge/Etch/ICP Metal Etcher|ICP]] using Chlorine chemistry or with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | ||
==Wet etching of Titanium== | ==Wet etching of Titanium== | ||