Specific Process Knowledge/Etch/Wet Platinum Etch: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch click here]''' | |||
Ething of Platinum can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | Ething of Platinum can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | ||