==Wet PolySi Etch==
==Wet PolySi Etch==


[[Image:BBHF-PolySi-Al-etch.jpg|thumb|Wet PolySilicon Etch (in the middle): positioned in cleanroom 4]]
[[Image:BHF-PolySi-Al-etch.jpg|thumb|Wet PolySilicon Etch (in the middle): positioned in cleanroom 4]]


The wet PolySi Etch is an isotropic silicon etch. This holds for both a poly-silicon thin-film as well as single-crystalline material such as a Si(100) surface. The PolySi Etch process is placed in a dedicated PP-tank in a laminar-flow bench in cleanroom 4.