UV Lithography uses ultraviolet light to transfer a pattern from a mask to a wafer coated with photoresist. The photoresist film is spin coated on the wafers and the pattern is transferred to the wafer by using a mask aligner. DTU Danchip houses a number of automatic or semi-automatic coaters and mask aligners.




Resist Overview

Resist Polarity Manufacturer Comments Technical reports Spin Coating Development Rinse Remover Process flows (in docx-format)
AZ5214E Positive AZ5214E.pdf‎ SSE, KS Spinner, III-V Spinner


AZ4562 Positive AZ4500.pdf‎ SSE, KS Spinner
AZ MiR 701 Positive AZ_MiR_701.pdf‎ Spin Track 1 + 2 Process_Flow_AZ_MiR701.docx‎
AZ nLOF 2020 Negative AZ_nLOF_2020.pdf‎ Spin Track 1 + 2 Process_Flow_AZ_nLOF_2020.docx‎


SU8 Positive KS Spinner