=== Shallolr === | === Shallolr === | ||
The shallolr recipe is designed to etch features (with sizes above 1 <math>\mu</math>m) in silicon down to a depth that ranges from a few microns to some 50 microns. If you need to etch deeper use Deepetch or more shallow, see Nanoetches. | The shallolr recipe is designed to etch features (with sizes above 1 <math>\mu</math>m) in silicon down to a depth that ranges from a few microns to some 50 microns. (If you need to etch deeper use Deepetch or more shallow, see Nanoetches.) It is specified to etch a 2 <math>\mu</math>m wide trench down to a depth of 20 <math>\mu</math>m on a wafer that has a global/local opening density of 10%. | ||
The recipe is given below. | The recipe is given below. | ||