Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Reactively sputtered SiO2 in Sputter-System Metal Oxide (PC1): Difference between revisions
Appearance
| Line 140: | Line 140: | ||
As it was mentioned earlier, the use of the Si target with the <b>oped dark space shield</b> leads to <b><span style="color: Coral">Cu</span></b> contamination, once the target gets old and heavily used. This is most likely due to the shrinkage of the target area. The XPS Cu 2p High-resolution scans reveal the difference in <b><span style="color: Coral">Cu</span></b> content in pure Si nonreactive sputtered film when an <b>open dark space shield</b> or <b>closed dark space shield</b> is installed. | As it was mentioned earlier, the use of the Si target with the <b>oped dark space shield</b> leads to <b><span style="color: Coral">Cu</span></b> contamination, once the target gets old and heavily used. This is most likely due to the shrinkage of the target area. The XPS Cu 2p High-resolution scans reveal the difference in <b><span style="color: Coral">Cu</span></b> content in pure Si nonreactive sputtered film when an <b>open dark space shield</b> or <b>closed dark space shield</b> is installed. | ||
<gallery caption="Figure 10. X-ray photoelectron spectroscopy." widths=" | <gallery caption="Figure 10. X-ray photoelectron spectroscopy." widths="400px" heights="350px" perrow="2"> | ||
image:eves_XPS_Cu_open_dark_space_shield_20210809.png| Cu 2p High-resolution scan in sputtered Si thin films using the <b>open dark space shield</b> and the seasoned (old and heavily used) Si target. | image:eves_XPS_Cu_open_dark_space_shield_20210809.png| Cu 2p High-resolution scan in sputtered Si thin films using the <b>open dark space shield</b> and the seasoned (old and heavily used) Si target. | ||
image:eves_XPS_Cu_closed_dark_space_shield_20210809.png| Cu 2p High-resolution scan in sputtered Si thin films using the <b>closed dark space shield</b> and the seasoned (old and heavily used) Si target. | image:eves_XPS_Cu_closed_dark_space_shield_20210809.png| Cu 2p High-resolution scan in sputtered Si thin films using the <b>closed dark space shield</b> and the seasoned (old and heavily used) Si target. | ||