==Non reactive SiO<sub>2</sub> deposition from SiO<sub>2</sub> target==
==Non-reactive SiO<sub>2</sub> deposition from SiO<sub>2</sub> target==


SiO<sub>2</sub> can also be sputtered directly from SiO<sub>2</sub> target with RF bias assistance in the Sputter-System (Lesker).
SiO<sub>2</sub> can also be sputtered directly from SiO<sub>2</sub> target with RF bias assistance in the Sputter-System (Lesker).