Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system: Difference between revisions
Appearance
| Line 236: | Line 236: | ||
The load-lock chamber is the only part of the tool which can be accesed by user. Ventilation and pumping takes approximately 5 min. The chamber has its own turbo pump. Inside there is a shelf - a cassete with 10 slots. The images below shows the load-lock set-up and sample mounting. The shelf is designed to handle 6-inch wafers, which has to be placed into dedicated carrier rings. Those rings with wafers can be introduced to the cassete - shelf. Different adapter-holders can be used for operating with 4-inch wafers and small chips. After the load-lock is pumped it takes approx. 6 min tol transfer the sample into the process chamber and 8 min to return back. | The load-lock chamber is the only part of the tool which can be accesed by user. Ventilation and pumping takes approximately 5 min. The chamber has its own turbo pump. Inside there is a shelf - a cassete with 10 slots. The images below shows the load-lock set-up and sample mounting. The shelf is designed to handle 6-inch wafers, which has to be placed into dedicated carrier rings. Those rings with wafers can be introduced to the cassete - shelf. Different adapter-holders can be used for operating with 4-inch wafers and small chips. After the load-lock is pumped it takes approx. 6 min tol transfer the sample into the process chamber and 8 min to return back. | ||
<gallery caption=" | <gallery caption="Cassette loader and sample mounling." widths="800px" heights="600px" | ||
00px" perrow="2"> | 00px" perrow="2"> | ||
image:Kaempe_Lesker_Load_Loak_image1.png| The load-lock chamber. | image:Kaempe_Lesker_Load_Loak_image1.png| The load-lock chamber. | ||