Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system: Difference between revisions
Appearance
| Line 202: | Line 202: | ||
== Sputter-System Metal-Oxide(PC1) == | == Sputter-System Metal-Oxide(PC1) == | ||
Chamber PC1 consists of six KJLC Torus® 3" magnetron sputtering sources with possibility of RF, DC, Pulse DC and HIPIMS sputtering. There are Argon, Nitrogen and Oxygen gas lines connected to this chamber. | |||
<gallery caption="Process chamber (PC 1)" widths="600px" heights="600px" perrow="2"> | <gallery caption="Process chamber (PC 1)" widths="600px" heights="600px" perrow="2"> | ||