Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Deposition of Silicon Oxide using LPCVD TEOS: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
[[Image:teos1.jpg|300x300px|thumb|Figure 1: TEOS structure]] | [[Image:teos1.jpg|300x300px|thumb|Figure 1: TEOS structure]] | ||
[[Image:teos2.jpg|300x300px|thumb|Figure | [[Image:teos2.jpg|300x300px|thumb|Figure 2: TEOS deposited in a trench etched in Silicon]] | ||
Danchip have one [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD furnace]] for deposition of TEOS: The furnace was installed in 1995 and can handle 4" wafers. It is furthermore possible to dope the TEOS with either Boron or phosphorous. | Danchip have one [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD furnace]] for deposition of TEOS: The furnace was installed in 1995 and can handle 4" wafers. It is furthermore possible to dope the TEOS with either Boron or phosphorous. | ||