[[Image:TEOS1.jpg|300x300px|thumb|Figure 1: TEOS structure]]
[[Image:teos1.jpg|300x300px|thumb|Figure 1: TEOS structure]]
Danchip have one [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD furnace]] for deposition of TEOS: The furnace was installed in 1995 and can handle 4" wafers. It is furthermore possible to dope the TEOS with either Boron or phosphorous.  
Danchip have one [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD furnace]] for deposition of TEOS: The furnace was installed in 1995 and can handle 4" wafers. It is furthermore possible to dope the TEOS with either Boron or phosphorous.