'''Test wafer position:''' Center of the boat
'''Test wafer position:''' Center of the boat


A better uniformity was achieved by annealing in N<sub>2</sub>. Measured film thickness was approximately 370 nm and the sheet resistance was measured to 200 [&Omega;<sub>sq</sub>] +/- 15 [&Omega;<sub>sq</sub>].
A better uniformity was achieved by annealing in N<sub>2</sub>. Measured film thickness was approximately 370 nm and the sheet resistance was measured to 200 &Omega/sq +/- 15 &Omega/sq.