Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of Silicon Nitride using PECVD: Difference between revisions
Appearance
| Line 35: | Line 35: | ||
|~32 | |~32 | ||
|1.89 | |1.89 | ||
| | |~1 | ||
| | | | ||
|- | |- | ||
| Line 35: | Line 35: | ||
|~32 | |~32 | ||
|1.89 | |1.89 | ||
| | |~1 | ||
| | | | ||
|- | |- | ||