|1SiN
|1SiN
|
|
Deposition rate in the middle of two wafers: '''49nm/min+-1nm/min'''
Deposition rate in the middle of two wafers: '''49nm/min+-1nm/min''' (2015-04-24 BGHE) <br>
In the middel: '''72.6-76.4 nm/min''' (2014-08-13 BGHE) <br>
In the middel: '''72.6-76.4 nm/min''' (2014-08-13 BGHE) <br>
Variation over 3 wafers: '''71.4-78.6 nm/min''' (2014-08-13 BGHE)