Specific Process Knowledge/Lithography: Difference between revisions
Appearance
No edit summary |
|||
| Line 252: | Line 252: | ||
===[[Specific Process Knowledge/Lithography/Characterization|Characterization]]=== | ===[[Specific Process Knowledge/Lithography/Characterization|Characterization]]=== | ||
===[[Specific Process Knowledge/Lithography/DirectLaserWriter|Direct Laser Writer]]=== | ===[[Specific Process Knowledge/Lithography/DirectLaserWriter|Direct Laser Writer]]=== | ||
==[[Specific Process Knowledge/Lithography/DUVStepper|DUV Stepper]]== | ==[[Specific Process Knowledge/Lithography/DUVStepper|DUV Stepper]]== | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#GammaSpinner|Gamma Spinner]] | |||
*[[Specific Process Knowledge/Lithography/DUVStepper#DUVStepper|DUV Stepper]] | |||
==[[Specific Process Knowledge/Lithography/EBeamLithography|E-Beam Lithography]]== | ==[[Specific Process Knowledge/Lithography/EBeamLithography|E-Beam Lithography]]== | ||
*[[Specific Process Knowledge/Lithography/EBeamLithography#Spinner|E-beam Spinner]] | |||
*[[Specific Process Knowledge/Lithography/EBeamLithography#EBeam|E-Beam]] | |||
*[[Specific Process Knowledge/Lithography/EBeamLithography#Development|Development]] | |||
==[[Specific Process Knowledge/Lithography/NanoImprintLithography|NanoImprint Lithography]]== | ==[[Specific Process Knowledge/Lithography/NanoImprintLithography|NanoImprint Lithography]]== | ||
==[[Specific Process Knowledge/Lithography/3DLithography|3D Lithography]]== | ==[[Specific Process Knowledge/Lithography/3DLithography|3D Lithography]]== | ||
Revision as of 15:01, 30 May 2013
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Available lithography methods at Danchip
There are a broad varity of lithography methods at Danchip. The methods are compared here to make it easier for you to compare and choose the one that suits your needs.
Comparing lithography methods at Danchip
| UV Lithography | DUV Lithography | E-beam Lithography | Imprint Lithography | Two photon polymerization Lithography | |
|---|---|---|---|---|---|
| Generel description | Generel description - method 1 | Generel description - method 2 | 3 | 4 | 5 |
| Pattern size range |
|
|
|
|
|
| Resist type |
|
|
|
|
|
| Resist thickness range |
|
|
|
|
|
| Typical exposure time |
2s-30s pr. wafer |
?-? pr. ? |
Depends on dose (in units of muC/cm2), estimate exposure time on sheet 2 of e-beam logbook |
? pr. wafer |
? pr. µm2 |
| Substrate size |
|
|
We have cassettes that fit to
Only one cassette can be loaded at time |
|
|
| Allowed materials |
|
|
|
|
|