Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions
Line 50: | Line 50: | ||
|10Å/s to 15Å/s | |10Å/s to 15Å/s | ||
|About 1Å/s | |About 1Å/s | ||
|About | |About 10 to 250 Å/s | ||
|- | |- | ||
|- | |- |
Revision as of 14:59, 8 May 2013
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | E-beam evaporation (PVD co-sputter/evaporation) | Electroplating (Electroplating-Ni/electrochemical deposition) | |
---|---|---|---|---|
Batch size |
|
|
|
|
Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean | None |
Layer thickness | 10Å to 1µm | 10Å to 1 µm | 10Å to 1000 Å | A few µm to 1400 µm |
Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s | About 1Å/s | About 10 to 250 Å/s |
Comment | Only very thin layers (up to 100nm). | Sample must be compatible with plating bath. Seed metal necessary. |