Specific Process Knowledge/Back-end processing/Laser Micromachining Tool: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Back-end_processing/Die_Bonder click here]''' | |||
<!-- Replace "http://labadviser.danchip.dtu.dk/..." wih the link to the Labadviser page--> | |||
==Laser Micromachining Tool [[Image:section under construction.jpg|70px]] == | ==Laser Micromachining Tool [[Image:section under construction.jpg|70px]] == | ||
| Line 9: | Line 12: | ||
The machine is located in the basement of building 346 under the cleanroom. | The machine is located in the basement of building 346 under the cleanroom. | ||
'''The user manual(s), user APV(s), technical information and contact information can be found in LabManager:''' | |||
<!-- remember to remove the type of documents that are not present --> | |||
<!-- give the link to the equipment info page in LabManager: --> | |||
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=299 The Logitech PM5 Polisher/Lapper in LabManager] | |||
It is equipped with 2 high power lasers: | It is equipped with 2 high power lasers: | ||
| Line 27: | Line 36: | ||
This shows the interior of the tool with optics, scannerheads and stage. | This shows the interior of the tool with optics, scannerheads and stage. | ||
[[File:Laser_Micromachining_Tool_stage_room_details.jpg|400px|thumb|Inside lasertool]] | [[File:Laser_Micromachining_Tool_stage_room_details.jpg|400px|thumb|Inside lasertool]] | ||
<br clear="all" /> | |||
Revision as of 11:34, 7 May 2013
Feedback to this page: click here
Laser Micromachining Tool 
The Laser Micromachining Tool is a microSTRUCT vario from the company 3D-Micromac AG.
It is currently only for internal use by Danchip personel for training. It will be public available some time during the first half year of 2013.
The system is able to produce micro structures in different kinds of materials like metals, ceramics, composite materials, etc.
The machine is located in the basement of building 346 under the cleanroom.
The user manual(s), user APV(s), technical information and contact information can be found in LabManager:
The Logitech PM5 Polisher/Lapper in LabManager
It is equipped with 2 high power lasers:
- a 50W picosecond laser that can emit light at 3 wavelengths: 355nm, 532nm and 1064nm and a
- a 100W nanosecond laser with a wavelength of 1064nm.

It consist of these main parts:
- Upper service way
- Manual front door
- Operating panel
- Machine's feet (adjustable)
- Left service way
- Electrical cabinet
This shows the interior of the tool with optics, scannerheads and stage.