Specific Process Knowledge/Etch/Etching of Silicon: Difference between revisions
Line 215: | Line 215: | ||
*Photoresist | *Photoresist | ||
| | | | ||
* | *Photo-, DUV- and e-beamresist | ||
*E-beam resist | *E-beam resist | ||
*Silicon Oxide | *Silicon Oxide | ||
Line 223: | Line 223: | ||
*Other metals if they cover less than 5% of the wafer area (ONLY RIE2!) | *Other metals if they cover less than 5% of the wafer area (ONLY RIE2!) | ||
| | | | ||
* | *Photo-, DUV- and e-beamresist | ||
*Silicon Oxide | *Silicon Oxide | ||
*Silicon Nitride | *Silicon Nitride | ||
*Aluminium oxide | *Aluminium oxide | ||
| | | | ||
* | *Photo-, DUV- and e-beamresist | ||
*Silicon Oxide | *Silicon Oxide | ||
*Silicon Nitride | *Silicon Nitride |
Revision as of 06:33, 22 April 2013
Etch of silicon can be done by either wet etch or dry etch. The standard setups for this here at DANCHIP are:
Wet etches:
Dry etches:
- Si etch using RIE1 or RIE2
- Si etch using ASE (Advanced Silicon Etch)
- Si etch using DRIE-Pegasus (Silicon Etch)
- Si etch using IBE/IBSD Ionfab 300
Comparison of KOH etch, wet PolySilicon etch, RIE etch, ASE etch and DRIE-Pegasus for etching of Silicon
KOH | PolySilicon etch | RIE | ASE | DRIE-Pegasus | |
---|---|---|---|---|---|
General description |
|
|
|
|
|
Possible masking materials |
|
|
|
|
|
Etch rate |
|
|
|
|
|
Size of substrate |
|
|
|
|
|
Batch size |
|
|
|
|
|
Allowed materials |
|
|
|
|
|
This Part is under construction
Feedback to this page: click here
Comparing silicon etch methods at Danchip
There are a broad varity of silicon etch methodes at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.
Wet etches:
Dry etches:
- Si etch using RIE1 or RIE2
- Si etch using ASE (Advanced Silicon Etch)
- Si etch using DRIE-Pegasus (Silicon Etch)
- Si etch using IBE/IBSD Ionfab 300
Compare the methods for Si etching
KOH Etch | Wet PolySilicon etch | RIE (Reactive Ion Etch) | DRIE-Pegasus (Silicon Etch) | ASE (Advanced Silicon Etch) | ICP Metal Etch | IBE/IBSD Ionfab 300 | |
---|---|---|---|---|---|---|---|
Generel description |
|
|
|
|
|
|
|
Possible masking materials |
|
|
|
|
|
|
|
Etch rate range |
|
|
|
|
|
|
|
Substrate size |
|
|
|
|
|
|
|
Allowed materials |
|
|
|
|
|
|
|