==Deposition of Silicon Oxide using LPCVD== | ==Deposition of Silicon Oxide using LPCVD== | ||
The LPCVD oxide you can deposit at DANCHIP is called TEOS oxide. It can be made in the [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD TEOS furnace]]. It is a batch process meaning you can run a batch of 13 wafers at a time. The deposition takes place at temperatures of 725 degrees Celsius. The TEOS oxide has good step coverage and hole filing/covering properties and the film thickness is very uniform over the wafer. We have two standard TEOS processes: One for depositing standard layers ~(0-1.5 µm) and one for deposition thick layers ~(1.5µm-4µm). The TEOS oxide has a dielectric constant very close to the one for thermal oxide (3.65 for TEOS). | The LPCVD oxide you can deposit at DANCHIP is called TEOS oxide. It can be made in the [[Specific Process Knowledge/Thin film deposition/B3 Furnace LPCVD TEOS|LPCVD TEOS furnace]]. It is a batch process meaning you can run a batch of 13 wafers at a time. The deposition takes place at temperatures of 725 degrees Celsius. The TEOS oxide has good step coverage and hole filing/covering properties and the film thickness is very uniform over the wafer. We have two standard TEOS processes: One for depositing standard layers ~(0-1.5 µm) and one for deposition thick layers ~(1.5µm-4µm). The TEOS oxide has a dielectric constant very close to the one for thermal oxide (3.65 for TEOS). | ||
*[[/Deposition of Silicon Oxide using LPCVD TEOS|Deposition of Silicon Oxide using LPCVD TEOS]] | |||
==Deposition of Silicon Oxide using PECVD== | ==Deposition of Silicon Oxide using PECVD== | ||
PECVD oxide can be deposited in one of the [[Specific Process Knowledge/Thin film deposition/PECVD|PECVD]] systems. You can run 1-3 wafers at a time depending on which one of the PECVD's you use. The deposition takes place at 300 degrees Celcius. This can be of importance for some applications but it gives a less dense film and the oxide is expected to have some hydrogen incorporated. The step coverage and thickness uniformity of the film is not as good as for the LPCVD TEOS oxide. PECVD oxide has excellent floating properties when doped with boron and/or phosphorus. Then it can be used ex. as top cladding for waveguides or encapsulation of various structures/components. In one of our PECVD systems (PECVD3) we allow small amounts of metal on the wafers entering the system, this is not allowed in the LPCVD and in the other PECVD (PECVD1). It is also a possibility to dope the silicon oxide with Germanium for altering the refractive index of the oxide. | PECVD oxide can be deposited in one of the [[Specific Process Knowledge/Thin film deposition/PECVD|PECVD]] systems. You can run 1-3 wafers at a time depending on which one of the PECVD's you use. The deposition takes place at 300 degrees Celcius. This can be of importance for some applications but it gives a less dense film and the oxide is expected to have some hydrogen incorporated. The step coverage and thickness uniformity of the film is not as good as for the LPCVD TEOS oxide. PECVD oxide has excellent floating properties when doped with boron and/or phosphorus. Then it can be used ex. as top cladding for waveguides or encapsulation of various structures/components. In one of our PECVD systems (PECVD3) we allow small amounts of metal on the wafers entering the system, this is not allowed in the LPCVD and in the other PECVD (PECVD1). It is also a possibility to dope the silicon oxide with Germanium for altering the refractive index of the oxide. | ||
*[[/Deposition of Silicon Oxide using PECVD|Deposition of Silicon Oxide using PECVD]] | |||
==Deposition of Silicon Oxide using sputter deposition technique== | ==Deposition of Silicon Oxide using sputter deposition technique== | ||
At DANCHIP you can also deposit silicon oxide using [[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]] sputter system. One of the advantages here is that you can deposit on any material you like. | At DANCHIP you can also deposit silicon oxide using [[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]] sputter system. One of the advantages here is that you can deposit on any material you like. | ||
*[[/Deposition of Silicon Oxide using Lesker sputter tool|Deposition of Silicon Oxide using Lesker sputter tool]] | |||
==Comparison of the methods for deposition of Silicon Oxide== | ==Comparison of the methods for deposition of Silicon Oxide== | ||
| Line 79: | Line 83: | ||
|- | |- | ||
|} | |} | ||