Specific Process Knowledge/Etch/Etching of Silicon Oxide: Difference between revisions
Appearance
| Line 108: | Line 108: | ||
There are a broad varity of silicon oxide etch methods at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs. | There are a broad varity of silicon oxide etch methods at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs. | ||
*[[Specific Process Knowledge/Etch/Wet Silicon Oxide Etch (BHF)|Wet Silicon Oxide Etch]] | |||
*[[Specific Process Knowledge/Etch/Wet Silicon | *[[/SiO2 etch using RIE1 or RIE2|Dry etch using RIE1 or RIE2]] | ||
*[[/ | *[[/SiO2 etch using AOE|Dry etch using AOE]] | ||
*[[ | *[[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE/IBSD Ionfab 300]] | ||
*[[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE/ | |||
==Compare the methods for Silicon Oxide etching== | ==Compare the methods for Silicon Oxide etching== | ||
Revision as of 16:38, 11 April 2013
Silicon oxide can be etched using either wet chemistry or dry etch equipment. Wet chemistry is mainly used to remove all the oxide on the surface (backside and front side) of a wafer or for isotrotropic etching. Dry etching etches anisotropic. It etches one side of the wafer at a time and can be used to etch structures with several masking materials.
Etch of silicon oxide can be done by either wet etch or dry etch. The standard setups for this here at DANCHIP are:
Wet etches:
Dry etches:
Comparison of wet Silicon Oxide etch and dry etches (RIE and AOE) etch for etching of Silicon Oxide
| Wet Silicon Oxide etch (BHF, SIO Etch (wetting agent), 5%HF) | RIE | AOE | |
|---|---|---|---|
| General description |
|
|
|
| Possible masking materials |
|
|
|
| Etch rate |
|
|
|
| Batch size |
|
|
|
| Size of substrate |
|
|
|
| Allowed materials |
|
|
|
This Part is under construction
Feedback to this page: click here
Comparing silicon oxide etch methods at Danchip 
There are a broad varity of silicon oxide etch methods at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.
Compare the methods for Silicon Oxide etching
| Wet Silicon Nitride Etch | BHF | RIE (Reactive Ion Etch) | AOE (Advanced Oxide Etch) | IBE/IBSD Ionfab 300 | |
|---|---|---|---|---|---|
| Generel description |
|
|
|
|
|
| Possible masking materials |
|
|
|
AOE
|
|
| Etch rate range |
|
|
|
AOE |
|
| Substrate size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
|