==Wet etching of Chromium==
==Wet etching of Chromium==
[[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
[[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this:
Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. You can see the APV [http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here] We have two solution for this:


# Commercial chromium etch (Chrome Etch 18). You can see the APV [http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here]
# Commercial chromium etch (Chrome Etch 18).  
# HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate  - 90ml:1200ml:15g - You can see the APV [http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here]
# HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate  - 90ml:1200ml:15g
Etch rate are depending on the level of oxidation of the metal.
Etch rate are depending on the level of oxidation of the metal.