Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this: | Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this: | ||
# Commercial chromium etch (Chrome Etch 18) | # Commercial chromium etch (Chrome Etch 18)You can see the APV[http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here] | ||
# HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate - 90ml:1200ml:15g - | # HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate - 90ml:1200ml:15g - You can see the APV[http://www.labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here] | ||
Etch rate are depending on the level of oxidation of the metal. | Etch rate are depending on the level of oxidation of the metal. | ||