Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE magnetic stack etch: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
=Etching magnetic stacks= | =Etching magnetic stacks= | ||
Magnetic stacks can be etched or more precisly milled in the Ion Beam Etcher (IBE). Below is presented some work done on milling stacks of magnetic layers. | Magnetic stacks can be etched or more precisly milled in the Ion Beam Etcher (IBE). Below is presented some work done on milling stacks of magnetic layers. | ||
==Results of Design of Experiments optimization of magnetic stack etching ([mailto:kristian.rasmussen@nanotech.dtu.dk Kristian Hagsted Rasmussen] spring 2011)== | ==Results of Design of Experiments optimization of magnetic stack etching ([mailto:kristian.rasmussen@nanotech.dtu.dk Kristian Hagsted Rasmussen] spring 2011)== | ||