| Line 43: | Line 43: | ||
*~?nm/min | *~?nm/min | ||
| | | | ||
*~ | *~50-200 nm/min (depending on features size and etch load and recipe settings) | ||
| | | | ||
*~30nm/min (not tested yet) | *~30nm/min (not tested yet) | ||