Specific Process Knowledge/Etch/Etching of Aluminium: Difference between revisions
Appearance
| Line 38: | Line 38: | ||
!Etch rate range | !Etch rate range | ||
| | | | ||
* | *~100nm/min (pure Al) | ||
| | | | ||
* | *~60nm/min (Al+1.5% Si) | ||
* | | | ||
* | |||
| | |||
* | |||
|- | |- | ||
| Line 38: | Line 38: | ||
!Etch rate range | !Etch rate range | ||
| | | | ||
* | *~100nm/min (pure Al) | ||
| | | | ||
* | *~60nm/min (Al+1.5% Si) | ||
* | | | ||
* | |||
| | |||
* | |||
|- | |- | ||