Specific Process Knowledge/Thermal Process/A1 Bor Drive-in furnace: Difference between revisions
No edit summary |
|||
| Line 1: | Line 1: | ||
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]= | |||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/A1_Bor_Drive-in_furnace click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/A1_Bor_Drive-in_furnace click here]''' | ||
==Boron Drive-in furnace (A1)== | ==Boron Drive-in + Pre-dep furnace (A1)== | ||
[[Image:A1.JPG|thumb|300x300px|A1 | [[Image:A1.JPG|thumb|300x300px|A1 Boron Drive-in + Pre-dep furnace. Positioned in cleanroom 2]] | ||
The Boron Drive-in furnane (A1) is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a pre-deposition and oxidation of the boron phase layer. Boron pre-deposition takes place in the | The Boron Drive-in + Pre-dep furnane (A1) is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a pre-deposition and oxidation of the boron phase layer. Boron pre-deposition takes place in the same furnace. The Boron Drive-in furnace can also be used for drive-in of boron which has been ion implanted. | ||
The Boron Drive-in furnace is the top furnace tube in the A-stack positioned in cleanroom 2. The A-stack | The Boron Drive-in + Pre-dep furnace is the top furnace tube in the A-stack positioned in cleanroom 2. The A-stack are the cleanest of all furnaces in the cleanroom. Please be aware of which substrates that are allowed to enter this furnace. Check [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 the cross contamination chart]. | ||
'''The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:''' | '''The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:''' | ||
Revision as of 15:16, 19 September 2013
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Boron Drive-in + Pre-dep furnace (A1)
The Boron Drive-in + Pre-dep furnane (A1) is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a pre-deposition and oxidation of the boron phase layer. Boron pre-deposition takes place in the same furnace. The Boron Drive-in furnace can also be used for drive-in of boron which has been ion implanted.
The Boron Drive-in + Pre-dep furnace is the top furnace tube in the A-stack positioned in cleanroom 2. The A-stack are the cleanest of all furnaces in the cleanroom. Please be aware of which substrates that are allowed to enter this furnace. Check the cross contamination chart.
The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:
Process knowledge
- Boron drive-in: look at the Dope with Boron page
- Oxidation: look at the Oxidation page
- Annealing: look at the Annealing page
| Purpose |
|
Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|