This furnace is used to grow oxide on metals or dirty wafers and to anneal wafers up to 1000 degree Celsius. | This furnace is used to grow oxide on metals or dirty wafers and to anneal wafers up to 1000 degree Celsius. | ||
Revision as of 13:44, 11 October 2013
Noble furnace
Feedback to this page: click here
This furnace is used to grow oxide on metals or dirty wafers and to anneal wafers up to 1000 degree Celsius.
The Noble furnace is located in service room 3.
The user manual, technical information and contact information can be found in LabManager:
Overview of the performance of the Noble Furnace
| Purpose | Oxide growth, annealing | |
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|